Developed to support the official Community Bureau of Reference (BCR) particle metrology standards |
|
|
|
Calibration for any method of particle size analysis | |
|
|
Specified traceablility - NIST, BCR and NPL standards | |
|
|
One of the largest International teams ever assembled | |
|
|
Unambiguous primary methods used - microscopy, sieving, sedimentation & the Coulter method | |
|
|
Seven standards covering the size range 0.1 - 2000mm | |
|
|
Produced as single shot vials from 25mg - 10g to minimise potential sampling errors during analysis |
For further information on each size, simply click on the appropriate button in the table below:
* Currency conversions are provided as a guide only and are therefore subject to slight fluctuation
|
|
People who visited this page were also interested in...
![]() |
![]() |
| TECHNICAL SPECIFICATION for soda-lime glass |
||
|
Physical Properties |
||
| Specific Gravity | 2.43 - 2.49 g/cm3 | |
| Refractive Index | 1.51 - 1.52 | |
| Hardness Mohs | 6 | |
| Rockwell | 47 RC | |
| OPH 50g load | 540 kj/mm2 | |
| Knoop 100g load | 517 kj/mm2 | |
| Coefficient of fraction | ||
| Static | 0.9 - 1.0 | |
| Dynamic | 0.7 - 0.8 | |
|
Mechanical Properties |
||
| Young Modules | 6.89 x 104 N/mm2 | |
| Rigidity Modulus | 2.96 x 104 N/mm2 | |
| Poissons ration | 0.21 | |
|
Electrical Properties |
||
| Volume Resistivity at 50Hz | 300 G.Ohm-m | |
| Dielectric Strength | 4500 kV/cm | |
| Dielectric Constant (at 1KHz) | 7.6 | |
| Power Factor | 0.9 | |
|
Thermal Properties |
||
| Softening Point | 740ºC | |
| Thermal Conductivity | 1.05 W/mK | |
| Expansion of Co-efficient | ||
| (0-300ºC) | 7.75 x 10-6/K | |
| Specific Heat | 770 J/kgK | |